There are plates available as X52 which's mills specially make for API pipes,
Essar was making plates marked as API X52, X80 etc. I have seen when I visited their plant long back.
It is difficult to get equivalent ASME/ASTM spec
Try the following
DIN 17006 StE 360.7, StE 360.7 TM
DIN 17007 1.0578 1.0582,
17172 EN 10208-2,
L360NB, L360MB, L360QB,
-----Original Message-----
From: S V [mailto: @
.com]
Sent: Monday, February 11, 2008 4:42 PM
To: Bathula Raghuram (Mumbai -
PIPING)
Subject: API 5L Gr X52
To get the above tubular rolled what plate material should be used.
Regards,
| "Bathula Raghuram (Mumbai -
PIPING)" <R.Ba...@ticb.com>
Sent by: material...@googlegroups.com 11/02/2008 07:34 PM
|
|
=======================================================
Confidentiality Notice
This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postm...@fwuk.fwc.com.
=======================================================