Dear expert

Can anybody tell me the meaning of qw 403.9
 for single pass or multipass welding  in which any pass is greater than 13mm thick, an increase in base metal thickness beyond 1.1 times that of the qualification test coupon.

Dhamodaran

unread,
Apr 1, 2014, 9:03:23 AM4/1/14
to material...@googlegroups.com
Dear Sandeep,

If the thickness of the single pass/run is more than 13mm,then the maximum qualified thickness will be restricted to 1.1 times of the coupon thickness.

Regards
Dhamodaran
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


kannayeram gnanapandithan

unread,
Apr 1, 2014, 10:09:03 AM4/1/14
to materials-welding
This is to control Heat input

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY

rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA

unread,
Apr 2, 2014, 1:38:09 AM4/2/14
to material...@googlegroups.com
Dear Sir,

This clause refers; for single pass and multi pass with 13mm and more deposition heat input increases and so base metal thk range is 1.1 times the qualified thk and such condition happens with SAW, GMAW, FCAW, SMAW processes only.