100 % NDE when No possible to perform pressure test

80 views
Skip to first unread message

Zakaria ghrab

unread,
Feb 3, 2017, 2:27:40 AM2/3/17
to material...@googlegroups.com
Dear Expert,

  Where we can find that Full NDE Volumic & Surfasic NDE for welded joints when is not possible to perform Pressure Test.

Construction code ASME B31.1

Thank you very much.

--

Thanks and Regards, 
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805


Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

dilintas

unread,
Feb 11, 2017, 9:38:18 PM2/11/17
to material...@googlegroups.com
Nowhere 



Sent from my Samsung Galaxy smartphone.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD8EeB1z0nR5vgoDBCiKwLspRV9QG50rNAPg1dKsHH0_Rc%2BPxA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

kausar khan

unread,
Feb 12, 2017, 7:29:00 AM2/12/17
to material...@googlegroups.com
Please refer 345.9 "Alternative Leak Test" B31.3


Kausar Kamal Khan


Dinesh Somwanshi

unread,
Feb 12, 2017, 8:13:15 AM2/12/17
to material...@googlegroups.com

100% Volumetric NDE in lieu of leak test is acceptable as per 31.3.

Thanking You,

With Regards..
Dinesh V Somwanshi
Api 570, Cswip 3.1,Bgas 2
Authorised Certified Piping, Welding, Painting Inspector.
00919881344135

On Feb 12, 2017 8:08 AM, "dilintas" <dili...@gmail.com> wrote:
Nowhere 



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Zakaria ghrab <zakari...@gmail.com>
Date: 02/02/2017 17:53 (GMT+02:00)
Subject: [MW:26005] 100 % NDE when No possible to perform pressure test

Dear Expert,

  Where we can find that Full NDE Volumic & Surfasic NDE for welded joints when is not possible to perform Pressure Test.

Construction code ASME B31.1

Thank you very much.

--

Thanks and Regards, 
-----
زكرياء غراب
GHRAB Zakaria 
Tunisia : +216 96 635 805


Yesterday is the past, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/sh8aes0gj2sdvc2rng849mwl.1486833533188%40email.android.com.

George Dilintas

unread,
Feb 12, 2017, 8:23:48 AM2/12/17
to Meghanadh K
which send you back to 345.8, which includes pressure test at lower pressures, but pressure test anyway

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1025218314.3028541.1486900648611%40mail.yahoo.com.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Pradeep kumar hormis

unread,
Feb 12, 2017, 9:22:37 PM2/12/17
to material...@googlegroups.com
Sir

Please refer ASME B 31.3 below:


345.9 Alternative Leak Test
The following procedures and leak test method may be
used only under the conditions stated in para. 345.1(c).
345.9.1 Examination of Welds. Welds, including
those used in the manufacture of welded pipe and fittings,
that have not been subjected to hydrostatic or
pneumatic leak tests in accordance with this Code, shall
be examined as follows:
(a) Circumferential, longitudinal, and spiral (helical
seam) groove welds shall be 100% radiographed in
accordance with para. 344.5 or 100% ultrasonically
examined in accordance with para. 344.6.
(b) All welds, including structural attachment welds,
not covered in (a) above, shall be examined using the
liquid penetrant method (para. 344.4) or, for magnetic
materials, the magnetic particle method (para. 344.3).

Thanks & Regards

PRADEEPKUMAR HORMIS



 
 


 

On Sun, Feb 12, 2017 at 4:15 PM, George Dilintas <dili...@gmail.com> wrote:
which send you back to 345.8, which includes pressure test at lower pressures, but pressure test anyway
Reply all
Reply to author
Forward
0 new messages