s355 pqr

25 views
Skip to first unread message

erich kuster

unread,
Feb 6, 2017, 5:40:01 PM2/6/17
to Materials & Welding
good day

can pqr on fillet to en 15614-1 be welded, if material used to weld pqr is s235. in other words
 paperwork says plate is s355 but s235 is used to do mock upp for pqr. same group no.

regards
erich

Tomas gonzalez

unread,
Feb 7, 2017, 6:45:27 AM2/7/17
to material...@googlegroups.com
No, yo have to weld base material with equal or minor yield strength of pqr base material  (and same group).
Just in case that you weld two diferents materials of same group at least one of them has to be equal or minor yield strength than pqr used base material. 

Regards 


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c0919461-8337-4ece-aaa6-d0d8546f8995%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages