Dear Experts ,
 
If the wleder is  qualifide for 6G test , can he weld the plate of  unlimited thickness ?
or he needs to Qualify 4G test to weld unlimited thickness of plate ?
 
wether the 6G welder is sapose to weld only pipes.
 

awaiting for  welding experts valueable  suggestions ..........

 

Regards

ABDUL JABBAR KHAN

Suresh

unread,
Jul 29, 2011, 12:19:39 AM7/29/11
to material...@googlegroups.com
Mr.Abdul ,
 
Your query is not clear ....Thickness qualification is  depends on weld cupon thickness , not depends on  Position ...
 
If the welder is qualified 6G Position then he can qualify any position but not any thickness..
 
Normally Sex IX , 2T is welder for thickness range qualification
 
Suresh

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

arvinda shan

unread,
Jul 29, 2011, 11:39:50 PM7/29/11
to material...@googlegroups.com
Dear Mr.Abdul,
 
6G is for position. If he qualifies in 6G position, he can do welding in any position . Reference.....SecIX- QW-461.9
 
For thickness, upto 13 mm thickness , he qualifies 2T. Beyond 13 mm , unlimited thickness.  Reference..... Sec IX -QW-452.1(b)
 
Regards
 
Arvinda.

kalyan vvv

unread,
Jul 30, 2011, 1:35:11 AM7/30/11
to material...@googlegroups.com
Dear abdul,
                if the welder qualifies in 6G position to maximum thickness (more than 13mm). that welder is qualified in 4G position on plate also upto maximum thickness.

THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
HYDERABAD
Mob.NO- 09885273257

Biplab Pal

unread,
Aug 1, 2011, 12:09:35 AM8/1/11
to material...@googlegroups.com
Dear KHAN,
 
Position is not related with thickness qualified.
For unlimited thickness qualification please refer QW 452.1(b) in sec IX 2007.


 
On Thu, Jul 28, 2011 at 7:32 PM, abdul khan <abdul_k...@yahoo.co.in> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Biplab Pal
Industrial Services, Inspection Engineer.
SGS India Pvt. Ltd.
Kolkata Branch
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

Karthik

unread,
Aug 1, 2011, 9:15:24 PM8/1/11
to material...@googlegroups.com
Hi,
If the welder qualified in 6G position with the pipe thickness(test specimen) is more than 13mm,then he qualified for pipe and plate of maximum to be welded.

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Mon, 8/1/11, Biplab Pal <bipla...@googlemail.com> wrote:
Reply all
Reply to author
Forward
0 new messages