what is the difference between d4 and d7 film

2,747 views
Skip to first unread message

baskar...@gmail.com

unread,
Feb 9, 2018, 5:33:54 AM2/9/18
to Materials & Welding
Dear Expects 

how to classify the d4 and d7 film , tell the difference between two films.

Thanks and Regards
Baskar P

james gerald

unread,
Feb 9, 2018, 6:20:33 AM2/9/18
to material...@googlegroups.com
D4 Films are Extra Fine grain Film with Very High Contrast associated with High Cost and more exposure Time.


D7 Films are Fine grain Film with High Contrast and High Speed.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

VINOD

unread,
Jul 25, 2019, 5:17:57 AM7/25/19
to Materials & Welding
after develop the film how to know


On Friday, February 9, 2018 at 4:50:33 PM UTC+5:30, gerr...@yahoo.com wrote:
D4 Films are Extra Fine grain Film with Very High Contrast associated with High Cost and more exposure Time.


D7 Films are Fine grain Film with High Contrast and High Speed.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Friday, February 9, 2018, 2:33:47 PM GMT+4, <baskar...@gmail.com> wrote:


Dear Expects 

how to classify the d4 and d7 film , tell the difference between two films.

Thanks and Regards
Baskar P

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Babur Khan

unread,
Jul 25, 2019, 8:37:56 AM7/25/19
to material...@googlegroups.com
Dear Mr.  Vinod,
It’s depends on manufacturing brand, generally on corners they mentioned or marked for D4 or D7 identification.

Muhammad Babur Khan
Sent from my iPhone
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/08e18dce-93fa-4e4e-80ea-2d93aa472f65%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages