When do we specify HIC requirements along with NACE Sour service requirements?
In many case NACE + HIC are mentioned...what does this mean?
stephen raj
unread,
Aug 2, 2023, 11:41:40 PM8/2/23
Reply to author
Sign in to reply to author
Forward
Sign in to forward
Delete
You do not have permission to delete messages in this group
Copy link
Report message
Show original message
Either email addresses are anonymous for this group or you need the view member email addresses permission to view the original message
to Materials & Welding
Fluid service or exposure to an oilfield environment containing Hydrogen Sulfide (H2S) can cause cracking of materials by damage mechanisms such as SSC / HIC / HSC / SCC /\ SOHIC / SWC / SZC.