Dear all

I want to weld cast iron with SS 304, Kindly advice for suitable electrode SMAW process 

Thanking you,


P.K.MAJI
Sr Surveyor,
BUREAU VERITAS (I) PVT LTD.,
e-mail:-prabi...@in.bureauveritas.com
NAGPUR,
www.bureauveritas.co.in
Mob:9422127912

Kannayeram Gnanapandithan

unread,
Jul 7, 2019, 11:16:54 PM7/7/19
to materials-welding
ENiCi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20190706053128.27434.qmail%40f5mail-224-127.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

George Dilintas

unread,
Jul 9, 2019, 11:18:08 PM7/9/19
to material...@googlegroups.com
Nickel electrodes

--

Vinay Thattey

unread,
Jul 16, 2019, 11:19:41 PM7/16/19
to material...@googlegroups.com
You can weld cast iron to steel using  Nickel electrode. The higher the carbon content, the lesser the weld ability. ... Cast iron is difficult, stresses are very high in weld , care to be taken , to weld.
Nickle electrodes such as Nickle 99 can be used . Check for joint design . Kindly See ANSI/AWS-A-5.15 .
Welding on cast iron may involves some repairs .

--

George Dilintas

unread,
Jul 17, 2019, 12:24:06 PM7/17/19
to material...@googlegroups.com
do buttering on cast iron before welding the pieces together


For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages