EEMUA 234 90/10 CU NI ASTM 466 UNS 70610 Vs UNS 7060X

336 views
Skip to first unread message

Inspection engineer

unread,
Dec 19, 2021, 6:16:53 AM12/19/21
to Materials & Welding
Greetings

Please kindly advise whether EEMUA 234 90/10 CU NI ASTM 466 UNS 70610 and UNS 7060X are same ?

what are the suitable filler materials required for welding ?

Regards
Viswa Manoj

pgos...@rogers.com

unread,
Dec 19, 2021, 8:17:57 PM12/19/21
to material...@googlegroups.com

Hi,

This grade of alloy is conventional 90/10 cupronickel. See the link below from the EEMUA webpage.

ASTM 466UNS 70610(Copper Alloy (UNS C70610) (azom.com)) is also of the same chemistry as that of the EEMUA grade. Refer the attached data sheet for guidance on welding fillers.

 

You may search in the web for additional resources on welding consumable manufacturers.

 

Thanks.

 

 

Pradip Goswami.P.Eng, IWE.

Independent  Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

EEMUA Publication 234 Digital

 

From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of Inspection engineer
Sent: December 17, 2021 8:42 PM
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:32689] EEMUA 234 90/10 CU NI ASTM 466 UNS 70610 Vs UNS 7060X

 

Greetings

 

Please kindly advise whether EEMUA 234 90/10 CU NI, ASTM 466 UNS 70610 and UNS 7060X are same ?

 

what are the suitable filler materials required for welding ?

 

Regards

Viswa Manoj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d55007b6-94c2-42d0-bde0-f401de7a75c2n%40googlegroups.com.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


D-70 Cupronickel rev 03.pdf