Gents,
 
To achieve sa-3 surface preparation grade using dry abrasive blasting method can we use sand as a abrasive?
Is any picture about this in the pictorial standard?
 

sathish sathish

unread,
Feb 10, 2010, 6:46:17 AM2/10/10
to material...@googlegroups.com
For SA 2.5 / SA 3, I recommend to use use grit blasting / shot blasting , if required a combination of both but not sand blasting. Nowadays, it is prohibited to use sand in blastng, as it  causes Silicosis, a lung disease, that is caused by the inhalation of toxic, carcinogenic crystalline silica dust particles. Silicosis is incurable and irreversible. 
 
Thanks
 
Sathish Rajkumar 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Reply all
Reply to author
Forward
0 new messages