to Materials-welding, MW, mirto....@gr.bureauveritas.com, Sedef Pala, pradip....@gmail.com, Pgoswami, george....@gr.bureauveritas.com, Amir Zakee Adnal, Meisam Shokri Arfaei, Murugesan Jeyaraman, Vino Varghese, tuan...@gmail.com, TDK YOKESH, Anup N. K. E., Umar Rashid Makrani, Pradip Kumar Sil, Jay Poojary, Venkatesan Mass Tech, John Henning, Lakshman, Mohammed Ismail, Hareesh K. V., Mohd Azam
Dear All,
Has any body qualified WPS based on AWS D1.4 to cover welds on pile cages as it was carried out in my site? the owner requested a qualified WPS to close this issue?
Your prompt action is highly appreciated.

MW

unread,
Sep 26, 2015, 11:45:17 AM9/26/15
to Materials & Welding
Dear Mostafa
Pl. don't send mails to individuals. Shooting off an e-mail to a person which you are not familiar will most likely be ignored. sending to the group ID in anyway will reach everyone in the forum

Thank you!

Mostafa Kamel Hussein

unread,
Sep 27, 2015, 2:33:15 AM9/27/15
to material...@googlegroups.com
OK and sorry for mistake



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7d12aa0a-33a5-4ca4-b3a0-b00057aca35c%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages