Personnel qualification to witness Sensitive Leak Test

41 views
Skip to first unread message

maheshQAQC

unread,
Sep 29, 2022, 11:38:16 PM9/29/22
to Materials & Welding
Dear Exerts,
is there any personnel qualification required as per SNT-C-1A to witness Sensitive Leak test as per B31.3 345.8 and ASME Sev-V Article 10 Appendix I.?
your valuable inputs are  highly appreciated thanks.

Mahesh

Pravin Kurade

unread,
Sep 29, 2022, 11:55:31 PM9/29/22
to material...@googlegroups.com
Please refer SNT TC 1A for qualification requirement 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/27f4a9be-aef1-4c60-9d85-406ccd8f958dn%40googlegroups.com.
--
Pravinkumar kurade
Reply all
Reply to author
Forward
0 new messages