Dear sir.
I saw one carbon steel MTC SA 537 CL 1 MTLTV ZT.

What is the explanation of MTLTV ZT.

Which source or code gives that explanation.
Kindly guide me.

Regards
venkat
trichy

----------
Sent from my Nokia phone

Kavin Murugam

unread,
Jun 28, 2012, 4:57:22 AM6/28/12
to material...@googlegroups.com
Dear Venkat,
 
Kindly refer SA20 ASME Sec II Part A.
MT=Heat treated
LTV=CVN done.
ZT= no idea
 
Kavin Murugam
0126159644
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Biswajit Mukherjee

unread,
Jun 28, 2012, 4:57:46 AM6/28/12
to material...@googlegroups.com
Pls. see ASME Sec II Part A : 2010 SA 20 Para 13.1.1, Para 12.1.7 and SA 770 Para 6.

In short: Heat Treated: low temperature Charpy V- notch impact tested: through thickness tension tested

Regards,





From:        "g.venka...@gmail.com" <g.venka...@gmail.com>
To:        "material...@googlegroups.com" <material...@googlegroups.com>
Date:        28-06-2012 13:54
Subject:        [MW:14709] Explanation of MTLTV ZT-Reg
Sent by:        material...@googlegroups.com




--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com

For more options, visit this group's bolg at
http://materials-welding.blogspot.com/

Saravanan Sornam

unread,
Jun 28, 2012, 8:49:52 PM6/28/12
to material...@googlegroups.com, kavin...@yahoo.com, g.venka...@gmail.com
Hi Friends,
 
I think ZT means,  Z direction Through Thickness tested.
 
Please clarify again.
 
Cheers,
Saravanan,
Korea