ASME B31.3 -2014 Table 331.1.1 Soaking time for P1 material

1,591 views
Skip to first unread message

SWI

unread,
May 29, 2017, 6:03:46 AM5/29/17
to Materials & Welding
Hi Team,

Could any please clarify
What is the minimum required soaking time for P1 material with wall thick 12mm, as per ASME B31.3 year 2014 Table 331.1.1 .

Is it still Minimum one hour per 1 Inch wall thickness or Minimum 15 Minutes...


Regards,

Ram

ASME B31.3-2004.pdf

MW

unread,
May 29, 2017, 6:26:38 AM5/29/17
to Materials & Welding
first of all, there is no necessity to attach code/std (or any copyright material) 

refer previous post [MW:591] Re: Copyright issues.

MK

unread,
May 31, 2017, 12:40:07 PM5/31/17
to Materials & Welding
For P no. 1 & 12 mm, the minimum soaking time for PWHT is 29 minutes & same is calculated from one hour per inch.

Also please note, the minimum 15 minutes in code, is for only if your value for minimum soaking time(after calculating from one hour per inch for respective thickness) is less than 15 minutes, for eg if you get 14 minutes then you should consider minimum 15 minutes.


Regards

Rajendra Jadhav

unread,
May 31, 2017, 11:50:14 PM5/31/17
to material...@googlegroups.com

Dear,
For your information the latest edition ASME B31.3 says there is no any requirements of PWHT.
If the wall thickness is more then will do preheat @95 Deg Celsius and which exemption of PWHT.

Regards,
Rajendra Jadhav

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

SWI

unread,
Jun 3, 2017, 6:04:20 AM6/3/17
to Materials & Welding
Hi Team,

Thanks for the Reply,

Seems for P1 material Minimum 1 hour soaking time requirement has been revised to minimum 15 minutes upto less than one inch wall thickness...
is there any code case on this issue... if there please share the number.

I am aware of PWHT exemptions. which are newly added in ASME B31.3 2014, however all those requirement are there in ASME Sec IX from long time..

Actually thought of attaching screen shot of Table T331.1.1, overlook attached 2004edition.

Regards,
RAM

Neem Lal

unread,
Jun 9, 2017, 12:31:55 PM6/9/17
to Materials & Welding
For P1 material up to 20 mm thickness no need PWHT.


On Monday, 29 May 2017 15:33:46 UTC+5:30, SWI wrote:

Ganesan

unread,
Jun 9, 2017, 11:29:22 PM6/9/17
to Materials & Welding

Dear Sirs

Kindly take a look
Auto Generated Inline Image 1
Reply all
Reply to author
Forward
0 new messages