ASTM A519 Gr.4130 - P No/ GP No. ? in ASME 2010 Ed.

3,430 views
Skip to first unread message

Kathalingam Babu

unread,
Nov 10, 2010, 2:28:44 AM11/10/10
to material...@googlegroups.com
Hi
 
Some one help me to have the P NO/GP NO for the above material in latest edition of ASME Sec IX
 
I don't have latest edition of ASME, as this material in earlier editions as unlisted one.
 
Thanks & Regards,
 
K.Babu
Singapore
 

Vikas Bhandari

unread,
Nov 10, 2010, 3:06:55 AM11/10/10
to material...@googlegroups.com
I have the latest dition of ASME SEC IX and ASTM SEC II PART A., but there is no a519 material with gr 4130 (qw 422 sec ix)

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

RAJAGOPAL KANNAN

unread,
Nov 10, 2010, 3:16:43 AM11/10/10
to material...@googlegroups.com
Dear Babu,
It does not fall under any P- No. or Group No.
This is an unassigned material.
If you are fllowing API 6A, 16 C codes, they allow to group yourselves with similar materials but not equivalent such as AISI 4140/ ASTM A 487 etc.
Thanks and Best Regards,
K.Rajagopal

--

george....@gr.bureauveritas.com

unread,
Nov 10, 2010, 4:44:15 AM11/10/10
to material...@googlegroups.com

neirther a Pno nor a Gr No is allocated to the Gr 4130

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04

limesh M

unread,
Nov 10, 2010, 5:43:39 AM11/10/10
to material...@googlegroups.com

 

Dear Mr. K.Babu,
 
I couldn't find the P No. and Gr. No of the material(ASTM A 519 Gr.4130) which you have mentioned in your query.The following ASTM A 519 Grades are listed in ASME BPV SEC IX, 2010 Edition.
 
 
Spec No

Type or Grade

UNS No.

Minimum specified tensile strength

Welding

Brazing

ISO 15608 Group

Nominal Composition

Product Form

P.No.

Gr.No.

P.No.

ATM A 519

1018HR 

G10180 

1

1

1

1.1

C

Tube

ATM A 519

1018CW

 G10180 

1

2

1

1.1

C

Tube

ATM A 519

 1020HR 

 G10200 

1

1

1

1.1

C

Tube

ATM A 519

1020CW

 G10200 

1

2

1

1.1

C

Tube

ATM A 519

 1022HR 

 G10220 

1

1

1

1.1

C

Tube

ATM A 519

1022CW 

 G10220 

70

1

2

1

1.1

C

Tube

ATM A 519

 1025 HR 

 G10250 

55

1

1

1

1.1

C

Tube

ATM A 519

1025CW 

 G10250 

75

1

2

1

1.2

C

Tube

ATM A 519

1026 HR 

 G10260 

55

1

1

1

11.1

C

Tube

ATM A 519

 1026 CW

 G10260

75

1

2

1

11.1

C

Tube

 
 
 
Regards,
 
Limesh

On Wed, Nov 10, 2010 at 11:28 AM, Kathalingam Babu <kathalin...@ppl.com.sg> wrote:

--

Kathalingam Babu

unread,
Nov 11, 2010, 1:11:18 AM11/11/10
to material...@googlegroups.com
Hi Limesh
 
Thanks for the info.
 
As per AWS B2.1 it is falls under M no.: 11B/ Gp no.: 9
 
Regards
 
K.Babu
Singapore

Easakimuthu Mookan

unread,
Jul 7, 2015, 4:17:32 AM7/7/15
to material...@googlegroups.com
Hi,

We have WPS for ASTM A519 Gr.4130 to 4130 and S355 to S355 , now we have an enquiry for 4130 to S355 welding , with our qualification we can do that job or not? anybody can answer

Rajagopal Kannan

unread,
Jul 7, 2015, 6:07:06 AM7/7/15
to material...@googlegroups.com
Dear Mohan,
Sorry. You have to qualify new WPS for the combination.
Thanks and Best Regards,
K.Rajagopal

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0de62087-ca9e-4a04-93a9-51b3cf0c7872%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

AbuT

unread,
Jul 23, 2015, 1:36:37 PM7/23/15
to Materials & Welding, rajagopa...@gmail.com
Hi all,

I have an enquiry for ASTM A519 Gr. 4130 Pipe. Some one please suggest me equivalent grade in API ( API 5L X52 / X60 ??? )


reg,
AbuT