Weld rejection rate for welders

721 views
Skip to first unread message

Ganesh R nair

unread,
Jun 11, 2023, 11:07:06 PM6/11/23
to material...@googlegroups.com
Dears,

As per SAEP - 324, linear weld rejection rate for welder is 0.2% max. But as per SAES W-10, maximum weld repair rate for welder is 2%. Which is correct. I am attaching screen shot of SAEP-324 and SAES W-10. Please advice.

Thanks & Regards,
Ganesh R
Screenshot_20230430-193444_Drive.jpg
Screenshot_20230430-191209_Drive.jpg

Pham Thanh Tinh

unread,
Jun 12, 2023, 1:03:00 AM6/12/23
to material...@googlegroups.com
Sir.

Targeted performance criteria on Weld Rejection Rate (WRR) for Welder and Welding Operator is 0.2% on linear method and 5% on weld joint method, with linear method being the over-riding factor. From the performance data the welders shall be categorized based on the linear Weld Repair Rate (WRR) as detailed in Appendix I. 

Vào Th 2, 12 thg 6, 2023 vào lúc 06:07 Ganesh R nair <ganesh...@gmail.com> đã viết:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ_8oJVEM1gb7b6ahL6ma0%3DndfA247w5OwNyOVKE73aidhdz3A%40mail.gmail.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


Kannayeram Gnanapandithan

unread,
Jun 12, 2023, 4:49:55 AM6/12/23
to material...@googlegroups.com
based on product like plates, 0.2%, For tubular products--2%
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--

Moossa Kutty

unread,
Jun 12, 2023, 4:50:03 AM6/12/23
to material...@googlegroups.com
This is misticken , actually 0.2 only

--

Kannayeram Gnanapandithan

unread,
Jun 12, 2023, 6:03:14 AM6/12/23
to material...@googlegroups.com
is it possible for manual welding

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

haas mread

unread,
Jun 14, 2023, 3:37:54 AM6/14/23
to material...@googlegroups.com
dear sir,

Please tell me where it is mentioned "based on product like plates, 0.2%, For tubular products--2%".