Request to suggest best welding electrode for SAE1018 to EN8

219 views
Skip to first unread message

M PRABAKARAN

unread,
Jan 9, 2024, 3:44:26 AM1/9/24
to Materials & Welding
Dear Sir,

Request to suggest best welding electrode for SAE1018 to EN8.

Regards,
M.Prabakaran
Trichy-India

Gopi Krishna Banerjee

unread,
Jan 24, 2024, 8:46:18 AM1/24/24
to material...@googlegroups.com
E-7018. Stick Electrode.

মঙ্গল, ৯ জানু, ২০২৪ তারিখে ২:১৪ PM টায় তারিখে M PRABAKARAN <pjk...@gmail.com> লিখেছেন:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3df42401-73ee-47a7-90d3-79039e1f39f4n%40googlegroups.com.

Prabakaran

unread,
Jan 25, 2024, 3:41:50 AM1/25/24
to material...@googlegroups.com
Thanks for feedback sir, Required any pre or post weld heat treatment.

 Regards,
M.Prabakaran
Trichy-India

You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/9UbEeHufuRo/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGhQL0k-9w_sAjEciPs7kn8KkWxSZHpOJWDNH%2BTL-6RbCeK0Lw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages