i have a wps for the material S275 JR in aws d1.1 (ITS AN UNASSINED MATERIAL IN AWS D1.1)                 Can i use this wps for welding ASTM A36  ANY WELDING ENGINEER IN THIS GROUPS PLEASE GIVE ME AN IDEA

hamed hammad

unread,
Jan 2, 2023, 2:32:20 AM1/2/23
to material...@googlegroups.com
asslam alikom 
if you have WPS  according to ASME IX  by using material S275 JR  this have ( P.NO.1 &GR.NO.1 ) in this case you can use it for welding  material ASME SA36   
IF you have material ASTME you shall determine the edition for know this in acceptance range ASME or not According to ASME SEC.II

‫في الاثنين، 2 يناير 2023 في 5:31 ص تمت كتابة ما يلي بواسطة ‪bavithran samuthralingam‬‏ <‪bavith...@gmail.com‬‏>:‬
Hi all 
i have a wps for the material S275 JR in aws d1.1 (ITS AN UNASSINED MATERIAL IN AWS D1.1)                 Can i use this wps for welding ASTM A36  ANY WELDING ENGINEER IN THIS GROUPS PLEASE GIVE ME AN IDEA

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0e8e5cc5-74e1-4c1c-9dd0-fd1bc79bed65n%40googlegroups.com.

james gerald

unread,
Jan 2, 2023, 3:46:33 AM1/2/23
to material...@googlegroups.com
S275JR is an EN code material and considered as Unlisted Material. According to AWS D 1.1 it will not permit to weld ASTM A36 material.

But in AWS D1.1 Engineer (Client) has an Authority over AWS D1.1 code  and can permit to use this WPS.

Please take the issue with the Client.

Some Snap shots of code provided below.

Inline image

Inline image





Inline image

Thanks & Regards

J.Gerald Jayakumar



On Monday, 2 January, 2023 at 09:01:04 am IST, bavithran samuthralingam <bavith...@gmail.com> wrote:


Hi all 
i have a wps for the material S275 JR in aws d1.1 (ITS AN UNASSINED MATERIAL IN AWS D1.1)                 Can i use this wps for welding ASTM A36  ANY WELDING ENGINEER IN THIS GROUPS PLEASE GIVE ME AN IDEA

--