Dear Experts,

Could you please clarify the mentioned subject, is it necessary to qualify the welders to perform the Temper Bead weld. If yes, what is the procedure/method for qualifying the welders.

Thank you,
Karthikeyan M
QA/QC Team 
Al-Muzain, Saudiarabia.

pgoswami

unread,
Dec 27, 2016, 12:01:52 AM12/27/16
to material...@googlegroups.com

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist.

Saudi Aramco Approved-Designated Project Welding Representative (DPWR).
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

H-905-9631505

C-905-9793232

 


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL7K%3D_%2BqTaAvJofJjv7KraxBMufM0ZmpsLPTpQ2%2BRSqKrzkrtw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

pgoswami

unread,
Dec 27, 2016, 12:05:35 AM12/27/16
to material...@googlegroups.com

Hi Karthikeyan,

 

The default rule is ASME Sec-IX, QW-290. If  the applications are for pipelines, then you need to follow the guidelines of Piping Research Council(PRCI) also as additional resource.

 

Where this technique would be applied, and what’s the grade of steel in question?

 

Appreciate your response.

 

Thanks.

 

 

 

Pradip Goswami, P.Eng,IWE


Independent Welding & Metallurgical Engineering Specialist.


From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Karthikeyan Muthuvel
Sent: Monday, December 26, 2016 7:02 AM
To: material...@googlegroups.com
Subject: [MW:25843] Welder performance for Temper Bead Welding

 

Dear Experts,

--

George Dilintas

unread,
Dec 28, 2016, 10:02:29 PM12/28/16
to Meghanadh K
You have to find the way through the labyrinth of QW-290 in ASME IX

2016-12-27 7:05 GMT+02:00 pgoswami <pgos...@quickclic.net>:

Hi Karthikeyan,

 

The default rule is ASME Sec-IX, QW-290. If  the applications are for pipelines, then you need to follow the guidelines of Piping Research Council(PRCI) also as additional resource.

 

Where this technique would be applied, and what’s the grade of steel in question?

 

Appreciate your response.

 

Thanks.

 

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthikeyan Muthuvel
Sent: Monday, December 26, 2016 7:02 AM
To: materials-welding@googlegroups.com
Subject: [MW:25843] Welder performance for Temper Bead Welding

 

Dear Experts,

 

Could you please clarify the mentioned subject, is it necessary to qualify the welders to perform the Temper Bead weld. If yes, what is the procedure/method for qualifying the welders.

 

Thank you,

Karthikeyan M

QA/QC Team 

Al-Muzain, Saudiarabia.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Loganathan M

unread,
Jan 10, 2017, 1:13:00 AM1/10/17
to Materials & Welding
Dear all,
               We have problem in aluminum welding Material is 5083 and filler matel is ER5556, Gas purity gas 99.999%

welding qualification getting major porosity. Please kindly give any precaution steps.

Kannayeram Gnanapandithan

unread,
Jan 10, 2017, 4:31:13 AM1/10/17
to materials-welding
use 5183 and mixture of Helium+Argon ( 75+25)

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, Jan 7, 2017 at 4:10 PM, Loganathan M <rml...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (rml...@gmail.com) Add cleanup rule | More info

Dear all,
               We have problem in aluminum welding Material is 5083 and filler matel is ER5556, Gas purity gas 99.999%

welding qualification getting major porosity. Please kindly give any precaution steps.

On Monday, 26 December 2016 15:03:48 UTC+3, Karthikeyan Muthuvel wrote:

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages