Dear All,

Whether Hardness test (PM/WM/HAZ) is mandatory for Welder qualification as per ASME Sec IX ?

Please provide the clause number if its required.

Thanking You,
Vikas Rana


safad pp

unread,
Feb 12, 2013, 6:42:24 AM2/12/13
to material...@googlegroups.com

Not required  for WPQ

Shafad P.P
Welding Inspector




--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

Reply all
Reply to author
Forward
0 new messages