WELD DISTANCE AS PER API 650

525 views
Skip to first unread message

Abd Ur Rehman

unread,
Aug 29, 2024, 5:36:10 AM8/29/24
to Materials & Welding
Daer expert what is the allowable distance between Vertical to Vertical & Horizantol to Horizantol Joints.

Mohd Siraj

unread,
Aug 31, 2024, 11:49:20 AM8/31/24
to Materials & Welding
refer api 650 section 7, its available.
before asking such straight question you could have refer code...
however there is no horizontal to horizontal value..only vertical offset..

Jobert Rappai

unread,
Sep 1, 2024, 5:55:02 AM9/1/24
to material...@googlegroups.com

In API 650, the allowable distance between vertical welds (also known as vertical joints or seams) in the shell of a welded steel storage tank is specified to prevent overlap of weld seams, which could affect the structural integrity of the tank.

According to API 650, Section 5.1.5.4:

  • The minimum distance between adjacent vertical weld seams on the same shell course should not be less than 3 times the thickness of the shell plate or 500 mm (20 inches), whichever is greater.

This requirement ensures that there is sufficient separation between vertical welds to avoid concentration of stresses and to provide adequate strength in the tank shell.

For example, if the shell plate is 10 mm thick, the minimum distance between vertical welds would be 30 mm (3 × 10 mm). However, since 500 mm is greater than 30 mm, the minimum allowable distance would be 500 mm.


On Thu, Aug 29, 2024 at 1:36 PM Abd Ur Rehman <khattakr...@gmail.com> wrote:
Daer expert what is the allowable distance between Vertical to Vertical & Horizantol to Horizantol Joints.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/be2f577d-7e81-4145-88ba-4ac272d94992n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages