Testing of heat resistant steel tubes PQR-ASME IX

40 views
Skip to first unread message

Dinesh K

unread,
Jul 23, 2025, 1:39:05 AM7/23/25
to Materials & Welding
Hi,

We are going to do PQR testing of heat-resistant steel tubes. Client has given a reference of QW-466.19 for the bend test, which i could not find in the latest ASME IX. 

Can anyone please help

sridhar cn

unread,
Jul 23, 2025, 6:35:21 AM7/23/25
to material...@googlegroups.com
If your client is referencing QW-466.19 in ASME Section IX for a bend test, it’s likely a misunderstanding o
misreference, as this clause does not appear in the 2017, 2021, or 2023 editions, nor in earlier editions.

Inform your client that QW-466.19 doesn’t exist in recent ASME Section IX editions on the intended clause or test 
requirements. We can proceed with standard bend test requirements under QW-466.1 (general bend test figures) 
and QW-163 (acceptance criteria).
C Sridhar.
-------------------------------------------------------------------------------------------------------------------------------------
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/732729f5-daa4-47f0-be88-367ad78c960bn%40googlegroups.com.

Vishwas Keskar

unread,
Jul 23, 2025, 11:51:25 AM7/23/25
to material...@googlegroups.com
What is ASME material grade?



--

K Dinesh

unread,
Jul 24, 2025, 5:16:04 AM7/24/25
to material...@googlegroups.com
ASTM A297 Gr. HP

Thanks & Regards

K.Dinesh 

Metallurgist


P.O. Box 1197, P.C 130, Muscat, Sultanate of Oman

Tel:  +968 24501524, 24505590 (Ext.42), Mob: +968 99880633, Fax: +968 24503814

Email: dinesh@lonestaralpha.com , Web: www.lonestaralpha.com , Location: Click here for Location Map

Locations: Muscat, Sohar, Duqm, Salalah & Liwa

Lonestar now does Pesticide Residues Testing in our new facility at Liwa!

 Consider your environmental responsibility. Think before you print.



sridhar cn

unread,
Jul 24, 2025, 5:16:04 AM7/24/25
to material...@googlegroups.com
 ASME uses and approves materials from ASTM and other sources for use in pressure-related applications, 
assigning them a special ASME designation (typically starting with “SA-”). These are called ASME-listed 
materials, but not "ASME grades".
In this sense, ASME does not invent material grades. but approves and lists them for use for the code applications.   
for example,
ASTM A516 → ASME SA-516
ASTM A240 → ASME SA-240.
Hope it is clear.
C Sridhar.
------------------------------------------------------------------------------------------------------------------------------------

sridhar cn

unread,
Jul 24, 2025, 8:56:40 AM7/24/25
to material...@googlegroups.com

ASTM A297 Grade HP (Cr 24-28% & Ni 33-37%) is a heat-resistant stainless steel casting alloy commonly used in high-temperature 

applications. ASTM A297 Grade HP (ASME sec II Part A and its UNS number is N08705) does not have a direct, one-to-one equivalent 

in ASME standards and modified slightly for specific applications (example: pressure vessels, piping).


For practical purposes, in ASME codes, Grade HP would be referenced under SA-297 Grade HP for applications like furnace parts, heat 

treatment equipment, or other high-temperature cast components. For a specific purpose like piping, it is referred to as ASME B16.5 -for 

flanges.


C Sridhar.

-------------------------------------------------------------------------------------------------------------------------------------------------