Dear all,

 

Can anybody elaborate chapter III of B31.3 regarding the impact test requirement of ASTM A333 where in section 323.2.2 states the limitation concerning impact testing  of a particular material. Is it mandatory for A333 to have an impact test ?,  where low temperature service is not an issue.

 

Your response are highly appreciated.

 

Regards,

 

Faigal Fernando Agbanawag
Sr. Piping Engineer
Clough ZFP

T +966 3 8828818 Ext: 241
F +966 3 8828622
M +966 (0) 507780576


Disclaimer: This email and any files transmitted with it are confidential and intended solely for the use of the addressee(s) named herein. If you are not the intended recipient or addressee, you should not use, disseminate, distribute, copy or alter this email. Any views or opinions presented in this email are solely those of the author and might not represent those of "CZFP".

Warning: Although reasonable precautions have been taken to ensure no viruses are present in this email, "CZFP" cannot accept responsibility for any loss or damage arising from the use of this email or attachments. If you have received this electronic mail message in error, please contact the sender directly.

piepe...@kpnmail.nl

unread,
Feb 26, 2009, 9:36:06 AM2/26/09
to Materials & Welding
Dear Sir,

I'm not familiar with the B31.3 but I know that all material according
to ASTM A333 have requirements for Impact testing for material
certification, except for Grade 11, see chapter 8 of ASTM A333 . This
means that all other material grades must have impact values mentioned
on their material certificate. Depending on the materials grade also
the test temperature is laid down in the ASTM A333, see table 5 of
this specification. The minimum requirements for each grade are
mentioned in table 4. Some grades even requires measuring lateral
expansion of the impact specimens. If it concerns welded pipe also
impact values are required for the weld area.
This is completely independent of the specification B31.3

If you can specify the grade of material I can send you the
requirements for this grade.

Best Regards,

Herman Pieper

On 26 feb, 13:06, "Faigal Fernando Agbanawag"
<faigal.agbana...@czfp.com> wrote:
> Dear all,
>
> Can anybody elaborate chapter III of B31.3 regarding the impact test
> requirement of ASTM A333 where in section 323.2.2 states the limitation
> concerning impact testing  of a particular material. Is it mandatory for
> A333 to have an impact test ?,  where low temperature service is not an
> issue.
>
> Your response are highly appreciated.
>
> Regards,
> Faigal Fernando Agbanawag
> Sr. Piping Engineer
> Clough ZFP
> T+966 3 8828818 Ext: 241
> F+966 3 8828622
> M+966               (0) 507780576        
>
> Disclaimer: This email and any files transmitted with it are confidential and intended solely for the use of the addressee(s) named herein. If you are not the intended recipient or addressee, you should not use, disseminate, distribute, copy or alter this email. Any views or opinions presented in this email are solely those of the author and might not represent those of "CZFP".
> Warning: Although reasonable precautions have been taken to ensure no viruses are present in this email, "CZFP" cannot accept responsibility for any loss or damage arising from the use of this email or attachments. If you have received this electronic mail message in error, please contact the sender directly.
>
>  czfp_Logo2.png
> 16KWeergevenDownloaden

Sridhar Doddapaneni

unread,
Feb 26, 2009, 10:37:35 AM2/26/09
to material...@googlegroups.com
Dear Faigal,

Yes, Impact test is mandatory requirement as per material specification of SA 333 Gr -  1,3,4, 6,7,9 & 10, even it is not designed for low temperature services.

Regards,

Sridhar Doddapaneni

pjo...@technip.com

unread,
Feb 26, 2009, 11:04:17 AM2/26/09
to material...@googlegroups.com
First of all, let me clarify that A333 material is intended for low
temperature service only. So it is unlikely that the material is not impact
tested except for grade-11

ASTM A333 calls for impact testing (except grade-11) as per the material
standard itself when the thickness exceeds 3 mm. (Refer Para-8 and
Table-5).

So far as the impact testing of material (as per design standard) is
concerned, I feel it is very well explained in Para 323.2.2(particularly
sub para a) and Table 323.2.2. Other/subsequent para's are also elaborative
for the exact requirement for various materials. Also, refer the Fig.
323.2.2A for other materials.

I hope this has clarified. As a matter of fact, I could not follow your
exact question. If you have any particular doubt, pl. specify otherwise, it
seems to be a hypothetical question.

Best regards,

Prasad




"Faigal Fernando
Agbanawag"
<faigal.agbanawag To
@czfp.com> <material...@googlegroups.com
Sent by: >
materials-welding cc
@googlegroups.com
Subject
[MW:1655] A333 Material for impact
26/02/09 04:06 PM test requirement


Please respond to
materials-welding
@googlegroups.com






Dear all,

Can anybody elaborate chapter III of B31.3 regarding the impact test
requirement of ASTM A333 where in section 323.2.2 states the limitation
concerning impact testing of a particular material. Is it mandatory for
A333 to have an impact test ?, where low temperature service is not an
issue.

Your response are highly appreciated.

Regards,



Faigal Fernando Agbanawag
Sr. Piping Engineer
Clough ZFP



T +966 3 8828818 Ext: 241

F +966 3 8828622

M +966 (0) 507780576









Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use,
disseminate, distribute, copy or alter this email. Any views or opinions
presented in this email are solely those of the author and might not
represent those of "CZFP".


Warning: Although reasonable precautions have been taken to ensure no
viruses are present in this email, "CZFP" cannot accept responsibility for
any loss or damage arising from the use of this email or attachments. If
you have received this electronic mail message in error, please contact the
sender directly.




Save a tree...please don't print this e-mail unless you really need to.







Save a tree...please don't print this e-mail unless you really need to.

Reply all
Reply to author
Forward
0 new messages