APPROVED WPS IN 2G POSITION BUT PRODUCTION WANT TO DO 5G/6G POSITION USING ASME 2G WPS

119 views
Skip to first unread message

Dominant QC

unread,
Jul 25, 2026, 4:21:50 AMJul 25
to Materials & Welding
Dear experts,

My contractors wants to use approved 2G position WPS for production joints which in 5G/6g position other than 2G position and WQT for 6G position. References to ASME. Can we proceed to do that or do we need to use approved WPS in 6G/ALL positions?

Regards,
Sya

Mohd Amiruddin

unread,
Jul 25, 2026, 4:28:05 AMJul 25
to material...@googlegroups.com
Can. Position is not a essential variables in ASME Sec IX. Can rewrite the WPS for ‘position: All.’

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/a2026e50-8b41-42a7-bd00-1852f82aa1ean%40googlegroups.com.

Dominant QC

unread,
Jul 25, 2026, 5:02:29 AMJul 25
to Materials & Welding
ok, i understand but they do not want to rewrite the WPS position to "ALL" because they said the position is non essential, they ignore it and they want proceed to use that 2G WPS for production/WQT. They are the stubborn contractor to deal with.

Jay Poojary

unread,
Jul 25, 2026, 5:03:43 AMJul 25
to material...@googlegroups.com
What is the weld process?

cordially,
Jay Poojary

--

Dominant QC

unread,
Jul 25, 2026, 5:57:48 AMJul 25
to Materials & Welding

Gtaw sir

Jay Poojary

unread,
Jul 25, 2026, 7:46:19 AMJul 25
to material...@googlegroups.com
Dear, 
If your WPS is established from ASME Sec IX, then please refer to Table QW-256 for GTAW Welding variables under QW-405.1, where addition of Position is a non essential variables, hence WPS can be rewritten for all positions & can be used on job.

cordially,
Jay Poojary

HITESH PATEL

unread,
Jul 25, 2026, 8:11:48 AMJul 25
to material...@googlegroups.com
Pl note, in WPS position is not essential variable hence same WPS can acceptable in any position however welder must be qualified 6G/5G with applicable group of materials qualification range as per applicable code. 


--

HITESH PATEL

unread,
Jul 25, 2026, 8:11:48 AMJul 25
to material...@googlegroups.com
It is ok. If vendor will not change position in WPS. Still you can use

sanket patel

unread,
Jul 25, 2026, 8:26:20 AMJul 25
to material...@googlegroups.com
Right. for Non Essential variables, you don't need to qualify the WPS/PQR. but even if variables is non essential, but you have to indicate that changes in WPS and need do revised it accordingly ASME SECTION 9.

sridhar cn

unread,
Jul 25, 2026, 3:12:04 PMJul 25
to material...@googlegroups.com

Under ASME Section IX, it is acceptable to use a WPS qualified with a 2G PQR for production welds 

made in 5G or 6G provided the WPS remains within its qualified essential variable ranges.

You do not need to qualify a separate WPS in 5G or 6G solely because production welding is in those 

positions.

However, the welders are to be individually qualified for the production welding positions like 5G and 6G. 

Otherwise, a contractor cannot use them other than in the 2G position. If the welder is qualified in 6G, 

Then he can weld in all positions, including fillets. 

C Sridhar.


--

sridhar cn

unread,
Jul 27, 2026, 7:49:52 AMJul 27
to material...@googlegroups.com
Please correct it to "welding positions like 5G (or) 6G"
Regret the typographical error. 
CS

Marco Nunes

unread,
Jul 27, 2026, 7:49:52 AMJul 27
to material...@googlegroups.com

Yes, under ASME Section IX, you can generally use a WPS that was qualified with a 2G procedure qualification test for production welding in 5G or 6G positions. You do not normally need to requalify the WPS in 6G/ALL positions.

The important point is that WPS qualification and welder qualification (WQT/WPQ) are two different things.

M Nunes



--

Ashishranjan - Domech Fabricators Pvt.Ltd.

unread,
Jul 27, 2026, 8:04:38 AMJul 27
to material...@googlegroups.com
Under ASME Section IX, it is generally permissible to use an approved 2G WPS for production welds made in 5G or 6G, provided the WPS is otherwise valid and all essential variables are satisfied. The critical requirement is that the welder is qualified for the production position (e.g., 6G). You do not normally need a separate WPS qualified in 6G or "all positions" unless required by the governing construction code or project specification.  

Regards,

Ashish Ranjan

Go green logo

Save a tree...Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hardcopy.



"Confidentiality Warning: This message and any attachments are intended only for the use of the intended recipient(s), are confidential and may be privileged. If you are not the intended recipient, you are hereby notified that any review, re-transmission, conversion to hard copy, copying, circulation or other use of this message and any attachments is strictly prohibited. If you are not the intended recipient, please notify the sender immediately by return email and delete this message and any attachments from your system.

Virus Warning: Although the company has taken reasonable precautions to ensure no viruses are present in this email. The company cannot accept responsibility for any loss or damage arising from the use of this email or attachment."


Caution: The e-mail below is from an external source. Please do not open attachments or click links unless this email comes from a known sender and you know the content is safe.



--

Marco Nunes

unread,
Jul 27, 2026, 8:04:41 AMJul 27
to material...@googlegroups.com
Noted.

This is a short table to easily check what is needed for each Item:

ItemQualificationProduction
WPS/PQR2G5G or 6G
Welder/WPQ6G5G or 6G
Result✅ Acceptable in principle

RANJITH ULAGANATHAN

unread,
Jul 27, 2026, 8:58:06 AMJul 27
to material...@googlegroups.com, material...@googlegroups.com
Dear All , 

Regarding All of Your Replies , I had An Questions
As Per Asme If you Want to Utilise the 2G WPS for 5G or 6G you Need to Additionally test the Bend test Coupon specimen to qualify the 6 G position  WPS , could Anyone Please Confirm How It’s Change from Your Answers 
WARM REGARDS
RANJITH

On 27 Jul 2026, at 3:04 PM, Ashishranjan - Domech Fabricators Pvt.Ltd. <plannin...@gmail.com> wrote:



Hai Tran Ngoc

unread,
Jul 27, 2026, 10:06:50 AMJul 27
to material...@googlegroups.com

Dear Mr.

All essential and nonessential variables specified in the WPS must be strictly followed. Once a variable is specified in the WPS, you are only permitted to perform the welding in accordance with that WPS. You can refer to QW-101; QW-200.1 for reference.




------------------------------------------------------------------
Hai, Tran Ngoc
Mechanical, Piping, Welding Inspector
Addr.: Binh Phu Ward, Ho Chi Minh City, Vietnam
------------------------------------------------------------------


Vào Thứ 2, 27 thg 7, 2026 lúc 19:58 RANJITH ULAGANATHAN <ulaganatha...@gmail.com> đã viết:

Hai Tran Ngoc

unread,
Jul 27, 2026, 10:06:52 AMJul 27
to material...@googlegroups.com

This means that if the WPS specifies only the 2G welding position, it may only be used for welding in the 2G position. If you want the WPS to cover all welding positions, the WPS must be revised accordingly (refer QW-203)



------------------------------------------------------------------
Hai, Tran Ngoc
Mechanical, Piping, Welding Inspector
Addr.: Binh Phu Ward, Ho Chi Minh City, Vietnam
------------------------------------------------------------------


Vào Thứ 2, 27 thg 7, 2026 lúc 20:52 Hai Tran Ngoc <ngoch...@gmail.com> đã viết:

Bharath Kumar

unread,
Jul 27, 2026, 11:42:27 AMJul 27
to material...@googlegroups.com
Hi,

you need to verify whether the supporting PQR for that WPS qualifies all required positions, the welding position used for PQR can be an essential variable for some welding processes. If the PQR was qualified only in 2G, it does not qualify the WPS for all welding positions. You must check the applicable essential variables for the specific welding process in ASME sec IX . 

BR
V.bharath

--

Kannayeram Gnanapandithan

unread,
Jul 28, 2026, 9:43:13 AMJul 28
to material...@googlegroups.com
For WPS, welding position is not an essential variable unless there is a requirement for Toughness. For Welders , Welding Position is an essential variable. 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 1090 & EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Sandeep Raghavan

unread,
Jul 28, 2026, 10:45:08 AMJul 28
to material...@googlegroups.com
Hai,

Please note that welding positions for procedure qualification is a non essential variable.
(in the Previous asme sec IX Editions, addition of position was a supplementary essential variable which is applicable only if toughness requirments applicable)

So if you qualify the PQR in any positions will qualify all positions.(for the welding process like GTAW, SMAW, FCAW, GMAW & SAW).

Regarding the performance qualifications, positions qualifications shall follow ASME section IX table QW 461.9.


With Regards,

SANDEEP RAGHAVAN







Reply all
Reply to author
Forward
0 new messages