Full form of WPB

3,254 views
Skip to first unread message

LOKNATH PATRA

unread,
May 3, 2012, 12:03:39 AM5/3/12
to material...@googlegroups.com

Dear experts,

            can anyone tell me for cs fittings material we use A234 Gr WPB.what is the full form of WPB & what is the carbon % in it.& other than that what grade can we use for cs fittings.

Regards
L.P

Suresh

unread,
May 4, 2012, 7:04:44 AM5/4/12
to material...@googlegroups.com
Dear Mr.LP

As I understanding that  ..

WPB Means .. Wrought Pipe Which is made from Weldable Pipe ,Grade B .Plz go through ASTM A 234 ,You can get % of Corbon details with respect to different grades .

Suresh

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 974 -  5 5 4 3 1 7 8 8  /  7 7 1 3 4 5 9 0 . ( Qatar )

 
                  91 - 92 92 905 905 ( India )

khatri ankit

unread,
May 5, 2012, 12:09:49 AM5/5/12
to material...@googlegroups.com
It means that Wrought Product Gr-B