A297 HD is a heat resistant casting alloy with 28Cr/5Ni.
I assume that in your project, welding of CS to A297 HD is for
structural purpose (welding supporting structure to casing etc). If it
is so, use E309L electrode and you will be fine.
If it is not a structural joint then please give us more information
about the service requirements.
Regards
Ramin Kondori
On 6/3/13, skroy <
sanje...@fivesgroup.com> wrote:
>
>
>
>
>
>
>
>
>
>
>
>
>
> dear all
>
> can you suggest suitable welding filler wire or electrode for welding of
> carbon steel (A106 Gr.B) and ASTM A297 HD material.
>
> thanks
> with regards
>
> --
>
>
>
>
>
>
>
>
> *Sanjeev Kumar Roy*
>
> Manager - QA/QC, BFC
>
> *Fives Combustion Systems Private Ltd.*
>
> Plot No- 230, Padra Jambusar Highway, Dabhasa
>
> Vadodara, Gujarat, 391440* - India*
>
sanje...@fivesgroup.com <mailto:
sanje...@fivesgroup.com>
>
>
www.fivesgroup.com <
http://www.fivesgroup.com/>
>
> Fives on Youtube <
http://www.youtube.com/groupfives>
>
>
>
>
> *This message and any attachments are confidential and for the sole
> attention of the addressees. Any unauthorized use or dissemination is
> prohibited.*
> Ce message et toutes pièces jointes sont confidentiels et à l'attention
> exclusive de ses destinataires.Toute utilisation ou diffusion non
> autorisée est interdite.
> *Please think about the environment before printing this e-mail.*//
> Merci de penser à l'environnement avant d'imprimer cet e-mail.
>
>
>
> --
> To post to this group, send email to
material...@googlegroups.com
> To unsubscribe from this group, send email to
>
materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
>
http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to
materials-weld...@googlegroups.com.
> For more options, visit
https://groups.google.com/groups/opt_out.
>
>
>
--
*Ramin Kondori*
*Sr. QA/QC Engineer
*
*SINOPEC*
r.ko...@petroyada.com
+98-2123592322
+98-9132150320