TUBE SELECTION IN HEAT EXCHANGER

32 views
Skip to first unread message

Ankit Gandhi

unread,
Jul 3, 2016, 9:20:45 PM7/3/16
to Materials & Welding
Dear sir,
 
I would like to know that what is criteria to select Tubes [Seamless or Welded] in heat exchanger ?
Which one is better as per strength?

Regards,
Ankit Gandhi

pgoswami

unread,
Jul 3, 2016, 10:36:39 PM7/3/16
to material...@googlegroups.com

Hello Ankit,

 

Seamless tubes would always be a better choice for any corrosive and demanding applications. This document provides general guidelines on the various differences between two types of tubes.

 

Thanks.

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist ,

Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ca0eed35-9269-459f-bbe7-7c1e4b9af2eb%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Seamless vs. Welded Tubing.pdf
Reply all
Reply to author
Forward
0 new messages