Dear experts,
I would appreciate your valuable response regarding the following inquiry.
The filler wire mentioned below is approved for our normal Gas Metal Arc Welding (GMAW) Welding Procedure Specification (WPS):
· AWS Classification: ER80S-G
· SFA Specification: 5.28
· API 1104 Group: 5
· Trade Name: PIPELINER 80Ni1
· Base metal API 5L Gr. X65
However, for repair welding joints, our approved WPS (GMAW Welding) specifies the use of the following filler wire:
· AWS Classification: ER80S-Ni1
· SFA Specification: 5.28
· API 1104 Group: 5
· Trade Name: PIPELINER 80Ni1
· Base metal API 5L Gr. X65
Unfortunately, my team used AWS Classification ER80S-G for the repair welding using Repair WPS.
I would like to know if this deviation is acceptable or if any corrective actions are necessary.
Thank you for your expertise and guidance.
Regards,
Baqer
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/30a48598-af6d-4f67-9b81-dcd6e1d9f3a1n%40googlegroups.com.

Thanks & Regards
J.Gerald Jayakumar