50 views
Skip to first unread message

Chandru Sekar

unread,
Sep 18, 2020, 6:24:18 AM9/18/20
to material...@googlegroups.com
I need details of furnace ...


Help to learn it ..


Entire things I want to know about furnace 


Thanks 
Chandru

Vishwas Keskar

unread,
Sep 18, 2020, 11:20:24 PM9/18/20
to material...@googlegroups.com
For what application 
1. Requirement 
2. Type of fuel
3.Size of job 
4.Temperatur of heat treatment
5. total type of heat treatments to be done 
PWHT .
, annealing etc 

there are so many variables before deciding the Furnace. 

Call furnace manufacturers.  they will prepare proposal to you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGWOcnqCbEPQJ_OLc9J9bPVz3DVWL0gFUpay9ui_Ls1JGhYY-A%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages