PTC as per IBR

243 views
Skip to first unread message

prateik tolani

unread,
Aug 25, 2020, 11:11:00 AM8/25/20
to material...@googlegroups.com
Dear Experts,

is PTC is compulsory as per IBR code.
give me reference.


Regards
Prateik

Kannayeram Gnanapandithan

unread,
Aug 26, 2020, 12:17:06 AM8/26/20
to materials-welding
Yea

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_AP0GK_QJmFgJMuQ7rHK1m97ohb2_0C6cc2Kr1CRHgeeA%40mail.gmail.com.

Kundan Ahirao

unread,
Aug 26, 2020, 12:17:06 AM8/26/20
to material...@googlegroups.com
Please refer IBR Regulation No. 561 a and b.

--


https://materials-welding.blogspot.com/


https://www.linkedin.com/groups/122787


---


You received this message because you are subscribed to the Google Groups "Materials & Welding" group.


To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_AP0GK_QJmFgJMuQ7rHK1m97ohb2_0C6cc2Kr1CRHgeeA%40mail.gmail.com.


--
Regards,
Kundan Ahirao

Dinesh Somwanshi

unread,
Aug 26, 2020, 12:17:06 AM8/26/20
to materials-welding
It's mandatory as per heat number & welder with process as well.

Regards

Dinesh

--

Kannayeram Gnanapandithan

unread,
Aug 26, 2020, 2:19:41 AM8/26/20
to materials-welding
ref IBR Regulation no. 561 & 257- For PTC

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349