orifice flange nipple seal welding & PT before hydro or after hydro hydro ?

275 views
Skip to first unread message

Amul Raj

unread,
Apr 2, 2016, 3:32:01 AM4/2/16
to Materials & Welding

 

 Dear Experts,


Our piping team prepared the orifice flange nipple seal welding & PT after hydro test

But, our client wants to install the nipple & seal weld before hydro test   

Which is the right method?

 

Regards,

Amul Raj T

Mohd Siraj

unread,
Apr 8, 2016, 12:14:54 AM4/8/16
to Materials & Welding
Before.


To ensure no leak during hydrotest.

Javeed Iqbal

unread,
Apr 18, 2016, 10:47:20 PM4/18/16
to material...@googlegroups.com
Before 
To ensure no leak 
On Thu, Apr 7, 2016 at 8:59 PM, Mohd Siraj <mohd...@gmail.com> wrote:
Before.


To ensure no leak during hydrotest.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f8a8c0b9-3470-40fc-bd5e-08588cd833c2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Arun Nair

unread,
Apr 19, 2016, 3:57:12 AM4/19/16
to material...@googlegroups.com

Dear Amul,
Need before hydro.

Arun nair.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

jaya anil

unread,
Apr 19, 2016, 3:57:33 AM4/19/16
to material...@googlegroups.com
If you have already welded the nipple after hydro test, go for re-hydro.

Thanks

--
Reply all
Reply to author
Forward
0 new messages