Request for Expert Advice on Crack Repair
I am writing to request the support of the experts out here on a crack repair in an exchanger. The exchanger has a fillet weld with the shell, and a crack was found during the last TAM. There is a possibility that the crack will be found again during this TAM.
The base material of the exchanger is 58mm P1 (A516-GR 70) with cladding of SS347 of 6mm. There are two scenarios to consider:
I would be grateful for any advice that you can provide on these two scenarios. Thank you for your time and consideration.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4010c4b0-e975-43fb-8399-b75840f3fc24n%40googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8b0c412-fb78-400e-91d2-7f29e17c934cn%40googlegroups.com.
![]() |
| |
TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies. The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments. | ||
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANRRH0JVz51_3StjR8FjHC_AGenZ8sqsfdsYiEFSJ8S22J1%2BEQ%40mail.gmail.com.