Hot tensile test at temperature 550 deg. celcius

25 views
Skip to first unread message

mechse...@gmail.com

unread,
Oct 8, 2015, 7:52:10 AM10/8/15
to Materials & Welding
Dear Experts,


Hot tensile test has given in ASME Sec II part D  upto 525°C for all material.

In our case design temperature is 550°C.(material 1.25Cr 0.5 Mo-Si  SA -335)

Question : what is the acceptable tensile/yield values above 525°C? (code allows only interpolation  not extrapolation)


Regards
Selastine Sudhakar