HARDNESS TEST

196 views
Skip to first unread message

Noel Tanilon

unread,
Jul 26, 2021, 12:07:31 AM7/26/21
to material...@googlegroups.com
Our Client is requesting hardness testing as mentioned in the equipment welding specification, where it stated the hardness test to be carried out on the following area for equipment which include tanks: 1. On Circumferential seam (some percentage) 2. Longitude seam (some percentage) 3. All temporary weld made and remove (100%) All the above requirements are so impractical to us since we are fabricating/erecting atmospheric tank (large diameters too). The amount of temporary weld (for erection purpose) are tremendous i.e. thousands for each crude oil storage tanks and hundreds on the miscellaneous tanks. The hardness test was carried out during the qualification of Welding Procedure Qualification and it meets the hardness value requirement. And there are no requirements for hardness tests as per API 650. I believe that it is meant for pressure vessel tanks only, but OWNER insists on the test since it is stated in the specification. Any comment on this client requirement? Please help.

Regards,

Noel
Noel C. Tanilon Jr
QA/QC Supervisor
Aboitiz Construction, Inc.
t 63 32 411 1800
m +63 917 849 8183
The information contained in this email message is intended for use only by the individual or entity to which it is addressed, and such information may be privileged, confidential and/or proprietary, and protected under applicable laws. 

Read about the full Aboitiz Disclaimer ( http://www.aboitiz.com/disclaimer)

JOEL REMOROZA

unread,
Jul 26, 2021, 9:32:28 AM7/26/21
to material...@googlegroups.com
Dear Noel,
Greetings!
Can you send the exact excerpt clauses from Client specification regarding hardness test.

Kind Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANff5sX-CKUrYid-4at6bYtKNN0SFLrsg%2Bw3kKfWK-uV4RdkEw%40mail.gmail.com.

Rishikesh Kumar

unread,
Jul 26, 2021, 9:32:29 AM7/26/21
to material...@googlegroups.com
Dear Noel,

This type of situation is most of the time faced by welding and quality engineers. For this reason quality assurance activities are performed prior to product realization. In this process basically all the documents are properly reviewed  and ensured for compliance for client requirements. we must review the documents - Technical/construction specification(API 650), client specification, client additional requirements and/or any other documents. based on these documents the quality Assurance/control plan is required to be prepared and subsequently approved from clients. once this QAP/QCP approved, further requirement shall be considered as additional requirement.

Being manufacturer,you may proceed in this way

1. if you realize this is impractical at this moment, you should request for non feasible activities at this moment.

2.perform the welding procedure qualification based for critical welding parement and show the results of hardness on test coupon.based on these results request for acceptance of production weld quality  and subsequently revise the PQR/WPS if required.
 
3. If feasible, and time permits, cost calculation shall be performed and  submit cost implication and subsequent time constraints.


Regards

Rishikesh kumar
Global Technical Support|Business Development|Lead Auditor|QA&QC|Welding| Pipe Mills|Steel Plants|Metallurgist

--