Welding Everhard C400/ Hardox 400 to SS304

57 views
Skip to first unread message

pkt...@gmail.com

unread,
Apr 10, 2021, 8:33:48 AM4/10/21
to Materials & Welding
We have project need to weld Everhard C400 to SS304. Please give me a hint on welding electrode to use, ER309 is a good choice?

Xuân Thông

unread,
Apr 10, 2021, 11:05:32 AM4/10/21
to material...@googlegroups.com
ER309 is okey

Vào Th 7, 10 thg 4, 2021 vào lúc 19:33 pkt...@gmail.com <pkt...@gmail.com> đã viết:
We have project need to weld Everhard C400 to SS304. Please give me a hint on welding electrode to use, ER309 is a good choice?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0b795cbe-87b4-4e85-b599-30e63532fe91n%40googlegroups.com.

Prem Nautiyal

unread,
Apr 10, 2021, 11:05:48 AM4/10/21
to material...@googlegroups.com
Use E309L.

Regards

Prem Nautiyal 


On Sat, 10 Apr 2021, 18:03 pkt...@gmail.com, <pkt...@gmail.com> wrote:
We have project need to weld Everhard C400 to SS304. Please give me a hint on welding electrode to use, ER309 is a good choice?

--

Aditya Gujar

unread,
Apr 12, 2021, 12:55:28 AM4/12/21
to material...@googlegroups.com
Hi,

According to Hardox website, you may use E309L or E307 type welding consumable. 

Regards,

Aditya Gujar



--
--
 
Aditya Gujar
Sales Manager
Essen Welding Alloys Pvt. Ltd.,
Pune, India.
 
Tel: 91 20 65781493
Mob: 91 9850958075
---