How to select equivalent grade material? A36 equivalent??

3,584 views
Skip to first unread message

Srinivas Engr

unread,
Jan 31, 2011, 8:52:34 AM1/31/11
to Materials & Welding
Dear All.
pl guide be about in selction of equivalent grade material?
Wat we have to look?
& In which spec we have to refer?
Wat r A36 equivalent materials..?
Wat about S275 grade material?


Thanks & Regards
Srinivas

Majid

unread,
Jan 31, 2011, 10:22:11 AM1/31/11
to Materials & Welding
Hi
At the first,it is important that the mechanical properties of chosen
material be the same,
the yield point and the tensile point of A36 is the same for all
thicknesses, But there is a little difference about the material
(Specially sheet metal) that is categorized by EN 10025 like s235
becuase the yield point of the s235 that is similar to A36 (almost)
is going down when the thickness is going up but the issue that is
very important is the Design assumptions.
I can send you the summarized properties of the materials if you want
but the final decision must be taken by the designer and accorting to
design assumption.

regards
M.R

vineet kumar

unread,
Feb 1, 2011, 8:46:14 AM2/1/11
to material...@googlegroups.com
Dear,

Question : Wat r A36 equivalent materials..?
Ans: IS Standard - IS: 2062 Gr.B

Regards,

Vineet

> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to materials-weld...@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

Plate Steel

unread,
Oct 30, 2015, 9:06:25 AM10/30/15
to Materials & Welding
Dear Srinivas,

Selection equivalent steel,you should mainly compare their chemical composition and mechnical property.

For checking A36,you can find specification ASTM A36/A36M.

A36 (Yield strength min.250Mpa,tensile strength at 400-550Mpa) is one most common carbon structural steel grade,the equivalent shall be EN 10025-2 S235JR,not S275JR,s275jr steel owned a higher tensile strength and yield strength than ASTM A36.

Else,Jis g3101 SS400 steel,DIN 17100 St37-2,GB /T700 Q235B steel and ASTM A283 Grade C are also similar with ASTM A36 steel.

Regards.

Eric from XINSTEEL INDUSTRIAL CO.,LIMITED

在 2011年1月31日星期一 UTC+8下午9:52:34,Srinivas Engr写道: