use of PN16 flanges dimensions are as per EN 1092-1 for asme div-1

26 views
Skip to first unread message

anthony chundal

unread,
Jul 27, 2016, 11:02:51 PM7/27/16
to Materials & Welding
Please advice whether we can use PN16 flanges dimensions are as per EN 1092-1 without providing any calculations as per appendix -2, for ASME Div-1 pressure vessel, material specification is SA105,

Hemant W Joshi

unread,
Jul 28, 2016, 1:51:08 AM7/28/16
to material...@googlegroups.com

What is the type of flange, size  in question?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6a44a704-4339-4191-a555-1ff396a4ab96%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------

anthony chundal

unread,
Jul 28, 2016, 2:13:09 AM7/28/16
to material...@googlegroups.com
the size is 1" & 2" WNRF sch 40.

dili...@gmail.com

unread,
Jul 28, 2016, 6:03:46 AM7/28/16
to Hemant W Joshi
If there the flange is not in accordance with one of the standards approved by the Code then calculation according App 2 us a must

Sent from my BlackBerry 10 smartphone.
From: Hemant W Joshi
Sent: Πέμπτη, 28 Ιουλίου 2016 - 08:51
Subject: RE: [MW:25152] use of PN16 flanges dimensions are as per EN 1092-1 for asme div-1

Reply all
Reply to author
Forward
0 new messages