SW-2.6 Performance Testing in ASME B16.20-2017

549 views
Skip to first unread message

MW

unread,
Nov 12, 2019, 3:28:41 AM11/12/19
to Materials & Welding
2017 edition Requires performance testing shall be conducted using an external calibration gas with a known methane concentration. Gasket filler thickness and density shall be determined by the manufacturer such that the performance testing criteria in para. SW-2.6 will be met. Q: Does anybody experienced deviation from gasket manufacturers? which laboratories are equipped with using Methane? Prior to 2017 edition this was not a requirement.

Vinay Thattey

unread,
Nov 18, 2019, 6:15:31 AM11/18/19
to material...@googlegroups.com
No Idea

On Tue, 12 Nov 2019 at 13:58, MW <raghura...@gmail.com> wrote:
2017 edition Requires performance testing shall be conducted using an external calibration gas with a known methane concentration. Gasket filler thickness and density shall be determined by the manufacturer such that the performance testing criteria in para. SW-2.6 will be met. Q: Does anybody experienced deviation from gasket manufacturers? which laboratories are equipped with using Methane? Prior to 2017 edition this was not a requirement.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d245dfe6-3b3f-4e65-a5aa-926b3a75c4da%40googlegroups.com.

Shashank Vagal

unread,
Nov 19, 2019, 12:29:33 AM11/19/19
to material...@googlegroups.com
Thanks, Vinay

Best Regards,

Shashank C Vagal (+91) 8082395502, 8779046302,