You can not reuse the electrode as it might be consumed . For better performance same flux
could be used for twice as it is after reheating then depend upon the condition of flux 60 /40
or 70/30 new / used you can use. used flux must be cleaned.
On Thu, 30 May 2013 09:02:04 +0530 wrote
--
>
To post to this group, send email to
material...@googlegroups.com
>
To unsubscribe from this group, send email to
materials-weld...@googlegroups.com
>
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
>
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>
---
>
You received this message because you are subscribed to the Google Groups "Materials &
Welding" group.
>
To unsubscribe from this group and stop receiving emails from it, send an email to materials-
welding+u...@googlegroups.com.
>
For more options, visit
https://groups.google.com/groups/opt_out.
>
>
>
Dear Sir,
Thanking You.
With Warm Regards,
Muthu barathi P,
Mobile No.
+918511180665Get your own
FREE website and domain with business email solutions,
click here