Welding Electrode Selection Table

442 views
Skip to first unread message

Venkatachalam Govindan

unread,
Jun 2, 2021, 8:19:38 AM6/2/21
to material...@googlegroups.com
Dear Respected Professionals, Gday.

We need a welding rod selection table, or suitable comparison table or the proper reference to select the electrode to any particular material if required. Hope our friends will help me. Thank you. All the best. 

Best Regards,
--
Venkatachalam Govindan
QHSE Lead | Auditor | Trainer
(API U Trainer | IRCA Lead Auditor | Exemplar Global MS Specialist |CQI Practitioner)
Mobile +965-97604989

Ramon Briceno

unread,
Jun 3, 2021, 12:24:11 AM6/3/21
to material...@googlegroups.com
Dear Venkatachalam,

Please consult the API 577 "Welding Processes, Inspection, and Metallurgy". It has information on electrode table and classification, of course there are many more, from welding technical firms, manufacturers, etc.

Regards, 
Ramon Briceño
Metallurgical Engineer.

Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: Venkatachalam Govindan <vin...@gmail.com>
Fecha: 2021/06/02 8:19 AM (GMT-04:00)
Asunto: [MW:32407] Welding Electrode Selection Table

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3OdqswNz6gvYtwT%2BUY%3DckN5MC%2BbqhzOMF-zMSqidvwXL-w%40mail.gmail.com.

Venkatachalam Govindan

unread,
Jun 3, 2021, 12:49:33 AM6/3/21
to material...@googlegroups.com
Thank you, dear Ramon, 

Yes, there is a lot, including ASME Sec.II, C. and Grouping in ASME Sec.IX, But, we need a proper reference like you said API 577 etc. 

Looking for other information too, for knowledge. All the best!

Regards, 

Venkat G.

james gerald

unread,
Jun 3, 2021, 2:48:05 AM6/3/21
to material...@googlegroups.com
Dear Mr.Venkatachalam,

Please refer to API RP 582.

Please also refer the below link.


Snap shot of the link below.

Inline image


Thanks & Regards

J.Gerald Jayakumar



--

james gerald

unread,
Jun 3, 2021, 2:48:07 AM6/3/21
to material...@googlegroups.com
Just to add,

Please refer attached for Pipeline welding.

Thanks & Regards

J.Gerald Jayakumar


On Wednesday, 2 June, 2021, 05:55:23 pm IST, Venkatachalam Govindan <vin...@gmail.com> wrote:


--
Welding+Consumables+For+Pipeline+Construction.pdf

Venkatachalam Govindan

unread,
Jun 3, 2021, 7:56:53 AM6/3/21
to material...@googlegroups.com
Thank you so much, dear, Gerald, for considering my request. All the best.

Venkat G.

james gerald

unread,
Jun 3, 2021, 10:12:13 PM6/3/21
to material...@googlegroups.com
Thanks  Mr. Venkatachalam,

The details provided by me gives only a guideline for selecting appropriate welding consumable based on suitability and matching chemical composition.

Apart from this there are various API, NACE, NiDL, SSA, Client specification and various Technical Articles which must be considered apart from the recommendation of ASME Sec.IIC based on Application such as Refinery, Natural Gas Plants, Petrochemical plants, Fertilizer plants etc. for Equipment and piping. It is always better to consult a Welding Engineer or Welding consultant/

Thanks & Regards

J.Gerald Jayakumar


Venkatachalam Govindan

unread,
Jun 7, 2021, 4:14:35 AM6/7/21
to material...@googlegroups.com
Thank you so much for your effort taken to write me a adequate information. I feel good and thankful Mr. Gerald. All the best. 

Best Regards,

Venkat G

--
--
Venkatachalam Govindan
Auditing & Training Manager
IRCA Registered Lead Auditor | API U Trainer |
CQI Practitioner | Exemplar Global CMSS
Kuwait +965-97604989 India +91-9840502376
Reply all
Reply to author
Forward
0 new messages