Eccentric Reducer (Fitting to fitting) Seam Orentation

76 views
Skip to first unread message

Dinesh

unread,
Jul 21, 2020, 8:54:44 AM7/21/20
to Materials & Welding
Dear all,

Eccentric Reducer (Fitting to fitting)  fit up, seam matching as below,
WhatsApp Image 2020-07-10 at 8.45.59 AM.jpeg

In this case,what is requirement need to follow and what is exact reason to do 1 inch. flushing on seam .

Thanks

Raja Varman

unread,
Jul 30, 2020, 7:50:14 AM7/30/20
to material...@googlegroups.com

Please discuss with client to get the actual situation approval.




என்றும் அன்புடன்,
Thanks & Regards,
RAJAVARMAN
+971561895584

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/baf9d41c-0489-493e-8699-7acebc37e5bdn%40googlegroups.com.

Dindo

unread,
Jul 30, 2020, 8:41:16 AM7/30/20
to material...@googlegroups.com
See UW-9(d), if you are using ASME Section VIII Div 1 as your construction code

--