Hello Experts

I`m looking for heat input formula for GTAW -Pulse- Hot wire process ,I got many different formula but  I can not trust to the references.
So would you please share your information about this subject with me .

Thanks every body  

pgoswami

unread,
Oct 29, 2015, 11:12:11 PM10/29/15
to material...@googlegroups.com

Hi Hamid,

 

Please see the extract from Sec-IX. Refer  Non Mandatory Appendix-H for more details in addition to QW 409. If the power source used is of Non Waveform type then QW-409 a,b or c may be followed. Follow 409.1 (b) or (c) for waveform controlled welding. You may choose one of the 3 stated formula below depending on the power source type. The original formula, QW-4091(a) is the baseline formula for all welding engineers. The other two  were adopted later.

 

Most precise way would be a combination of QW-409.1(a) & QW-409.1(C)-(2)

 

 

The ASME Section IX heat input measurement methods in QW-409.1(a) and QW-409.1(b), were developed at a time when welding power source output was relatively constant.

 

QW-409.1(c) more accurately reflects heat input changes when performing waveform controlled welding, but is also suitable for non waveform controlled (conventional) welding.

 

Thanks.

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist

Hamilton, Ontario, Canada

pgos...@quickclic.net

pradip....@gmail.com

ca.linkedin.com/pub/pradip-goswami/5/985/299

 

QW-409.1(a)

 

QW-409.1(C)-(1)

 

 

QW-409.1(C)-(2)

 


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/78f62b8c-f629-4bb1-a8d2-ce2c1e4c0b21%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

image001.gif
image002.gif
image003.gif
Reply all
Reply to author
Forward
0 new messages