Regarding WPS Heat Input.

744 views
Skip to first unread message

Prashun Kumar

unread,
Apr 3, 2014, 8:58:29 AM4/3/14
to material...@googlegroups.com
Dear All,
 
As In site,

 

Welding Inspector taking daily welding  parameters per pass each day   for WPS-01, currently for root, the welder is not able to meet the requirements of Min heat Input mentioned in the WPS.

For example :As per WPS

For root:

Amperage:84-102

Voltage:25.5-31.2

Travel Speed:3.35-4.10.

Heat Input(Min):0.710

 

Welder welding in current: 85, Voltage:27, Travel speed:3.36, Heat Input:0.68 which is not meeting the min Heat Input range.(whether this should be accepted or rejected).Please clarify.

   

 Reply given by -Welding Engineer in blue:   I suggest to increase the current  to slighter higher value without changing the voltage & travel speed.

 

    Mr.Mani, we need to try best combination of parameters by varying current, voltage & travel speed within the parameters provided in WPS      which are most suitable for all the welders in production welds.

 

     Once you fix the particular Amps, Volts, travel speed, you need to check these parameter in actual production whether welders are           

     following the same.  In above example, i feel just by increasing the current slightly will solve your problem.

 

Minimum variable range for amperage and voltage mentioned in the WPS is not meeting to achieve Min heat Input mentioned. If it is not achieving the Min heat input ,then why ranges for voltage and amperage  mentioned to follow the procedure.

This was asked to  QA/QC Inspectors, they were unable to clarify.

 

    WPS parameters are +/- 10% of PQR average values. 

 

   For getting min heat input, we should not multiply min current X min voltage/ Min Travel speed.

 

   If we use above formula in writing WPS ranges, WPS parameters will not be actual paramters used in PQR qualification.
 
 
 
 
Can anybody can clarify this for me: I m not satified with this answer :Can  anbody explain me how the parameters are taken from PQR to make WPS.
 
Regards,
 
Prashun

Prakash Hegde

unread,
Apr 3, 2014, 9:58:11 AM4/3/14
to material...@googlegroups.com
Hi!
I presume you are using SMAW process
and for SMAW process it is better  to use min bead length welded per unit length of electrode burnt during PQR qualification instead of controlling A  ,V and welding speed which is more fluctuating and difficult to control the speed of welding , A and V which depends upon arc length by welder
Regards
Hegde P.b.
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Dindo

unread,
Apr 3, 2014, 9:22:26 AM4/3/14
to material...@googlegroups.com
I am assuming that the travel speed is 3.36 inch/min which is
equivalent to 85.344 mm/min

Formula is VA X 60 / TS X 1000
85(27) X 60 / 85.344 X 1000 = 1.6 KJ

I am not sure where you got the 0.68 from.

Prashun Kumar

unread,
Apr 3, 2014, 10:48:21 PM4/3/14
to material...@googlegroups.com
Dear Dindo,
 
Travel speed is 3.36 mm/sec,its not in mm/Min,
 
 
Dear Hegde,
 
Process is SMAW.(Downhill welding)
 
 
Regards
Prashun