Re: [MW:17286] WHAT IS THE DIFFERENCE BETWEEN E7015 AND E7016,E7018

1,101 views
Skip to first unread message

kannayeram gnanapandithan

unread,
Apr 4, 2013, 2:26:11 AM4/4/13
to material...@googlegroups.com
yes,if not impact, but 7015 will have deep penetration charactership than others
Pandithan
welding Consultant

On 4/3/13, Elavarasan Dharma <sacet....@gmail.com> wrote:
> DEAR SIR,
> CAN I USE INSTEAD OF E 7016,E 7018 INSTEAD OF E 7015.
>
> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-weld...@googlegroups.com.
> For more options, visit https://groups.google.com/groups/opt_out.
>
>
>

Binoy Soman

unread,
Apr 4, 2013, 4:30:45 AM4/4/13
to material...@googlegroups.com
Dear Elavarasan,

Attached excerpt from AWS A 5.1 may be helpful for you

S.Binoy
Pages from AWS A5.1 (1991).pdf

Ahmad el-sharkawy

unread,
Apr 4, 2013, 9:48:35 AM4/4/13
to material...@googlegroups.com
E7015   electrode coating ( basic, low hydrogen, sodium)  penetration ( medium )  current type ( DCEP )
E7016   electrode coating ( basic, low hydrogen, Potassium)  penetration ( medium )  current type ( AC & DCEP )
E7018   electrode coating ( basic, low hydrogen, Iron powder)  penetration ( medium )  current type ( AC & DCEP )