Hi Chaitanya,
Can you ask this query in the group as I am unable to do so.
Any calculation sheet or method available for Thickness calculation for Blind Flange for 64 “ CS pipeline hydrotest.(test pr of 83 barg), 400# rating.
I had referred to one of the Client spec, which demands 170mm thick plates for the same.
Any reference of Agency or Consultant doing these kind of Calculations.
Thanks and regards,
Mithun
Design Engineer - Piping
Dodsal Engineering & Construction Pte. Ltd.
Dubai, U.A.E.
Phone : +9714-3161279
Use UG 34 of ASME Section VIII Div 1
--
ARUNACHALAM.A
050-5257122
Happiness Keeps You Sweet,
Trials Keep You Strong,
Sorrow Keeps You Human,
Failure Keeps You Humble &
Success Keeps You Glowing,
But Only Faith & Attitude Keeps You Going
| Chaitanya Purohit <chaitany...@yahoo.co.in>
Sent by: material...@googlegroups.com 09/27/2009 07:06 PM
|
|
Hi Chaitanya,
Thanks and regards,
Mithun
Design Engineer - Piping
Dubai, U.A.E.
Phone : +9714-3161279
Disclaimer :This email and any files transmitted with it are intended solely
for the use of the addressee(s) only and may contain confidential and/or
privileged information. If you are not the addressee, then this message
is not intended for you and be advised that you have received this email
in error and that any use , dissemination , forwarding, printing or copying
of this email is strictly prohibited. In such case please notify the sender
and delete this email and any attachments with it from your system immediately.Receipt
of this email by you shall not give rise to any liability on the part of
Larsen & Toubro Limited
| CARBON STEEL | ||||||
| - INPUT DATA - | INCH UNIT | METRIC UNIT | ||||
| 1. | MATERIAL | : | ASTM A515 GR.70 | |||
| ALLOWABLE STRESS(by B31.3) | : | 23100.00 | Psi | 1624.00 | ㎏/㎠G | |
| 2. | CORROSION ALLOWANCE (C) | : | 0.05 | inch | 1.30 | mm |
| 3. | PIPE QUALITY FACTOR(carbon은 1) | : | 1.00 | 1.00 | ||
| 4. | DESIGN PRESSURE(Kg/cm2G) | : | .00 | Psi | 57.00 | ㎏/㎠G |
| 5. | DESIGN TEMPERATURE( ℃) | : | .00 | 75.00 | ||
| 6. | FLUID | : | ||||
| - OUTPUT DATA - | ||||||
| 1. | The equation for wall thickness calculation based on ASME B31.3 | |||||
| tm = dg√(3P/16SE) + C | ||||||
| where, | ||||||
| tm : minimum required wall thickness in mm. | ||||||
| dg : inside diameter of gasket for raised or flat face flange or the gasket | ||||||
| pitch diameter for ring joint and fully retained gasketed flanged | ||||||
| E : joint efficiency or pipe quality factor | ||||||
| P : design pressure | ||||||
| S : allowable stress = ㎏/㎠ | ||||||
|
c : sum of allowance defined in para. 304.1.1
Using this formula the Thickness caluculates to 152.5 mm , Try for yourself if this could be helpful. | ||||||