distance between nozzle weld and circum. weld.

42 views
Skip to first unread message

emre pekince

unread,
Oct 23, 2020, 9:56:54 AM10/23/20
to material...@googlegroups.com
Hi, 

 I would like to check the distance between nozzle weld and circumfenetial weld of our products which design code is Asme Sec VIII div.1.
where can I find the tolerances or requirements?

thanks in advance

Sankaran Sp

unread,
Oct 24, 2020, 8:58:22 AM10/24/20
to material...@googlegroups.com
Dear friends,

During Stellite -6 hard facing (by TIG welding or Plasma welding) on Inconal alloy ( 825) . Is it required to follow pre heating ? & is it required PWHT process after welding? kindly give me your suggestion or answer to proceed further.  

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore,India. 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEm%2BGRW%2BSAYiQ4q8cdnBXEYHrBF1yLV4BujbVt9xiTNsyF1_eQ%40mail.gmail.com.

George Dilintas

unread,
Oct 30, 2020, 9:06:36 PM10/30/20
to material...@googlegroups.com
Read UW-14 

--