Required WPS for Martensite with CS

55 views
Skip to first unread message

Mostafa Kamel

unread,
Aug 8, 2023, 11:34:29 PM8/8/23
to material...@googlegroups.com

Hi Guys

I have 12Cr13 (Equivalent to martensitic stainless steel)  with Q355B (equivalent to ASTM A572 Grade 50)

Has any one WPS covered welding of above two materials?


BR


Vishwas Keskar

unread,
Aug 8, 2023, 11:42:21 PM8/8/23
to material...@googlegroups.com
Pl. furnish below 
1. Carbon steel % in Martensitic Steel 
2. Share MTC in Martensitic Steel 
3.What is the thickness?
4. What are service conditions
5 Is this pressure part or non pressure part 
6 Code of construction 

Thanks 
Vishwas 
IWE



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVihNKCFpiJvHKJHmOjuEns4VtGXpQKn8Rf_aEO4Rxhq4qqw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages