Regarding PT & MPI test on overhead position

643 views
Skip to first unread message

khatri ankit

unread,
Aug 5, 2011, 3:24:39 AM8/5/11
to Materials & Welding
Dear Experts,

I just want to know that in overhead position which NDT method is
suitable either DPT or MPI

Kindly mention the significance for the same.

y it's used ? and y it;s not used?

Regards,

Ankit Khatri

Pieper QSI

unread,
Aug 5, 2011, 3:48:34 AM8/5/11
to material...@googlegroups.com
Dear Sir,

You can apply both technologies in the overhead position. There are no
restrictions for these technologies regarding execution position.

Met vriendelijke groeten / Best Regards

Herman Pieper

Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl

-----Oorspronkelijk bericht-----
Van: material...@googlegroups.com
[mailto:material...@googlegroups.com] Namens khatri ankit
Verzonden: vrijdag 5 augustus 2011 9:25
Aan: Materials & Welding
Onderwerp: [MW:12112] Regarding PT & MPI test on overhead position

Dear Experts,

Regards,

Ankit Khatri

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to
materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

khatri ankit

unread,
Aug 5, 2011, 6:37:03 AM8/5/11
to material...@googlegroups.com
but sir in PT , it works on capillary action, due to overhead position, how it works? may u explain me plz how the penetrant draws in to the discontinuity, there is gravitation force.  

Pieper QSI

unread,
Aug 5, 2011, 7:07:12 AM8/5/11
to material...@googlegroups.com

You are correct regarding capillary working of PT. But the capillary attraction force of the PT liquid in cracks is greater than the gravitation force therefore you only will face some small gravity problems during application of the liquid, once the fluid is on the surface the natural adhesion and capillary forces will do the job.

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

khatri ankit

unread,
Aug 5, 2011, 8:04:28 AM8/5/11
to material...@googlegroups.com
thank u sir, n may u explain me how the MPI is done in overhead position?

Pieper QSI

unread,
Aug 5, 2011, 5:59:30 PM8/5/11
to material...@googlegroups.com

Contrast paint will be applied first if oil based MPI fluid is used with black iron particles. After that you can apply the MPI fluid during empowering the electrical magnet. Here also the fluid will stay on the surface due to natural adhesion of the oil based fluid. Perhaps you need to apply some extra MPI fluid compared to the horizontal position but there will be no problem detecting indications if these are present.

Eswaran samikannu

unread,
Aug 6, 2011, 9:19:35 PM8/6/11
to material...@googlegroups.com
Hi,
Overhead position you can apply PT conveniently,In MT during apply magnetic particle you face some problem ie fall over inspector. In PT you  use Solvent removable method you can eliminate .
Thanks
Regards
S.Eswaran
ASNT NDT Level III (PT,UT,RT&MT)
0065-83495961


From: Pieper QSI <piepe...@kpnmail.nl>
To: material...@googlegroups.com
Sent: Friday, 5 August 2011 3:48 PM
Subject: [MW:12113] RE: 12112] Regarding PT & MPI test on overhead position
materials-welding+unsub...@googlegroups.com

For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com

Eswaran samikannu

unread,
Aug 6, 2011, 9:25:42 PM8/6/11
to material...@googlegroups.com
PT works on basic principle of Surface tension & contact angle only major play, Gravity force not at all.
Thanks
S.Eswaran


From: khatri ankit <nids01...@gmail.com>
To: material...@googlegroups.com