shall we refer ASME sec VIII div-1 for soaking hours of normalising & tempering process-reg

80 views
Skip to first unread message

Sankaran Sp

unread,
Feb 22, 2022, 11:00:18 PM2/22/22
to Materials & Welding
Dear friends,

We used to get A217 - WC6 & A217 -WC9 casting from foundry with  normalising & tempering conditions, these details are given the MTC of the product. while checking the soaking hours for normalising & tempering process, they used to follow 4 hours for all 100 to 200 thickness jobs, when as asked to maintain 5 hours for 125mm, 6 hours for 150mm & 8 hours for 200mm thickness, they refused to increase the soaking hours from 4 hours and asking the reference standard for soaking hours, in this situation shall we refer ASME sec VIII div-1 for soaking hours w.r.to P nos? kindly help me in this regards.      .    


Regards,
Sankaran.SP
Coimbatore, India. 

Karthik

unread,
Feb 23, 2022, 12:07:59 AM2/23/22
to Materials & Welding
Hi,
For materials, we have to refer ASME Sec.II Part-A , SA217 and SA703 - S22.
S22. Heat Treatment
S22.1 Test specimens shall be heat treated together
with the castings they represent. Heat-treated specimens
shall be tested and shall meet the tensile and impact properties
specified.
S22.2 The remaining test specimens from Supplementary
Requirement S22.1 representing the casting shall be
treated thermally after the final (foundry) heat treatment
to simulate heat treatments below the critical temperature
that the casting may receive during fabrication, and then
tested for mechanical properties. Time, temperature, and
cooling rate shall be as stated in the order. In the case of
postweld heat-treatment, the total time at temperature or
temperatures for the test material shall be at least 80% of
the total time at temperature or temperatures during actual
postweld heat-treatment of the fabrication of which the
casting or castings are a part. The total time at temperature
or temperatures for the test material may be performed in
a single cycle. When this Supplementary Requirement is
specified, the welding qualification test metal must be processed
in the same manner.


Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2118283400.531862.1645459089014%40mail.yahoo.com.

Shahil Saini

unread,
Feb 23, 2022, 1:34:56 AM2/23/22
to material...@googlegroups.com
hello sankaran 

For the above mentioned casting material, refer to the images attached. And In ASME Sec II Part-A, SA217 & SA703 there is not any mentioned detail that for the above materials you can use ASME Sec VIII Div-1, But As per P-No. and G-No. you can refer UCS-56, in that Table UCS-56-3 and UCS-56-4 (please kindly read the general notes).

Thanks and regards
Shahil Saini
PGET-Welding



--
HT2.JPG
HT1.JPG
IX.JPG

Shahil Saini

unread,
Feb 23, 2022, 1:35:09 AM2/23/22
to material...@googlegroups.com
Cont'd with my above mail


HT3.JPG

Prakash Hegde

unread,
Feb 23, 2022, 2:07:08 AM2/23/22
to material...@googlegroups.com
Hi!
For Normalising you can not refer SecIII div 1 as it is referred to Pwht which is below AC1 temp

While as normalsing is carried above AC3 which depends upon component chemistry And final req mech 
properties to be achieved with metallographic requirement This is being established by heat treatment trials by product  mfgr
That is why mafgr is reluctant to change HT cycle
In such.case one has to accept recommended  HT cycle
Regards
Hegde
--

George Dilintas

unread,
Feb 23, 2022, 11:06:48 PM2/23/22
to material...@googlegroups.com
Yes you could refer to VIII-1

--
Reply all
Reply to author
Forward