Please advise the suitable filler wire to weld between SS to SS without purging.structural work. 
With regards. 
Saji Jos Purathoor. 

Kannayeram Gnanapandithan

unread,
Apr 25, 2020, 12:38:29 AM4/25/20
to materials-welding
Electrode for SMAW available with leading consumables manufacturers

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKZDJ1eUB_%2BqE9NENL067b_7u9Eu5_Be-1syzeSuAndOY7zJpg%40mail.gmail.com.

james gerald

unread,
Apr 25, 2020, 1:41:41 AM4/25/20
to material...@googlegroups.com
Try Kobe Japan, TGX Filler wires.

Thanks & Regards

J.Gerald Jayakumar




Vinay Thattey

unread,
Apr 27, 2020, 12:23:04 AM4/27/20
to material...@googlegroups.com, saji...@gmail.com
Ccan U be a bit specific .  Type /  grade / MOC i.e  SS 304 , 316 , 321 etc .  I assume its a plate material of say say ASTM-A-240 .